Flexural Damage Tester
A rectangular strip of coated fabric is wrapped around two opposite cylindrical positions, so that the sample is cylindrical. One of the cylinders reciprocates along its axis. The coated fabric tube is alternately compressed and relaxed, thereby causing folds on the specimen. This folding of the coated fabric tube continues until a predetermined number of cycles or significant failure of the sample occurs.
Comply with ISO7854,GB/T12586-B method, BS3424:9
1 | Fixture | 6 groups |
2 | Speed | 8.3Hz±0.4Hz(498±24r/min) |
3 | Cylinder | outer diameter 25.4±0.1mm |
4 | Test trajectory | arc R460mm |
5 | test stroke | 11.7±0.35mm |
6 | Clamp | width 10±1mm |
7 | Inner distance of clamp | 36±1mm |
8 | sample size | 50×105mm |
9 | Volume | 40×55×35cm |
10 | Weight | about 35kg |
11 | Power supply | 220V 50Hz |
Die Cutter: 1 piece
Power cable: 1 piece
RIGHT has helped customers in more than 100 countries to be successful and earn good profits. We also welcome you to become an exclusive distributor in your country.
After signing the agreement, we will not wholesale any more products to your country or region, your orders will be processed and shipped first, and we will execute your custom machine design after you send us the first time. Click the buttons below, and let’s grow your brand together.
No more endlessly wasting time on other lousy suppliers. RIGHT's goal is to let you sit back and relax. We take care of all the dirty works, including trade stuff, clearance and logistics, etc. Our consultant will keep you informed of the trade progress throughout.
We will contact you within 1 working day, please pay attention to the email sales@dgright.com